superalloys n. 超合金;超耐热不锈钢(superalloy的复数)
- The double shear specimen was designed for the study of the creep behavior of nickel base single crystal superalloys at high temperature.
双剪切试样是设计用于研究镍基单晶超合金的蠕变问题。 - H. Q. Ye, D. X. Li and K. H. Kuo: Tetrahedrally close-packed phase in superalloys, New phases and domain structures, Acta Metallurgica Sinica, 22 (1986), A1 - A43.
叶恒强,李斗星,郭可信:高温合金中的拓扑密推相:析相及畴结构,金属学报,22(1986),A1 - A43。 - In this paper, the influence of various deformation temperature, deformation degree and deformation velocity on structure and properties of superalloys in forging process was discussed.
本文讨论了在锻造过程中不同变形温度、变形程度、变形速度对高温合金组织和性能的影响。